Coalescence Voids

Coalescence Voids

CoalescenceVoidsCAUSES: Painting when the air or surface temperatures are too cold for the paint to form a film. Painting in non-heated areas. Surfaces deeply chilled need a heating period before painting. Surfaces temperatures  must be 50 degrees F or above.

 

SOLUTIONS: Avoid painting interior or exterior surfaces when the temperatures are too cold. Late afternoon painting in unheated areas are vulnerable because the temperature will continue to decrease during the right prevent proper paint film formation.

  • All
  • Adhesive
  • Algae
  • Bleeding
  • Blistering
  • Brick
  • Bubbles
  • Burnishing
  • Caulking
  • Cedar Stains
  • Ceiling
  • Chalking
  • Checking
  • Coalescence Voids
  • Concrete
  • Cracking
  • Curling Edges
  • Defects
  • Discoloration
  • Doors
  • Dry Applicator
  • Dye Bleed
  • Edges
  • Exterior
  • Exterior Walls
  • Flaking
  • Floors
  • Interior
  • Metal
  • Mildew
  • Patching
  • Pattern Matching
  • Peeling
  • Rust
  • Shading
  • Stains
  • Surface Preparation
  • Tears
  • Wallcoverings
  • Wall Coverings
  • Windows
  • Wood
load more hold SHIFT key to load all load all